With infusion, unless you're using 'Profinish' fabric that has the resin binder to help hold it together, then apply a light mist of spray-tack before cutting.
Something like Cytec's 'Aerofix 3' will work well.
I use an Olfa roller cutter, which does give nice clean cut lines when jointing pieces together and if you try and put your overlaps into corners, you can do a really good job of minimising the appearance of any joins
|