Hi,

I want to make a repair on a two stroke jet ski carbon exhaust system. 
The exhaust operates to a maximum of 90-95°C since it is constantly water cooled.
I believe I need an epoxy system that will withstand these temperatures.

I thought this would do the job: 
https://www.easycomposites.co.uk/el160-high-temperature-epoxy-laminating-resin

What I do not know is, at what extent do I get the temperature resistance, without post curing.
The system is supposed to be ok up to 180°C after full post curing, but how will it behave without it, since I do not have an oven this big in hand.

Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
500w work lights are your friend... 