Hi just a quick question

I have read up and watched your tutorials but still a little unsure on how long I should leave the coupling coat and the light weight matt ply to cure before moving onto the main heavy plies with uni-mould tooling resin.

Regards
Ian
Reply
Porkster0
Porkster0
Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)
Group: Forum Members
Posts: 14, Visits: 69
Hi Hanaldo and Warren

Thanks for the replys I am in no rush just didn't want to leave it too long !

so basically when it has hardened off it is ready to lay up,

Regards

ian
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search