Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Uni mould coulping coat
Uni mould coulping coat
Post Reply
Like
5
Uni mould coulping coat
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Porkster0
Porkster0
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 14,
Visits: 69
Hi just a quick question
I have read up and watched your tutorials but still a little unsure on how long I should leave the coupling coat and the light weight matt ply to cure before moving onto the main heavy plies with uni-mould tooling resin.
Regards
Ian
Reply
Like
5
Reply
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
You can move on as soon as it is hard.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Uni mould coulping coat
Porkster0
-
9 Years Ago
You can move on as soon as it is hard.
Hanaldo
-
9 Years Ago
Hanaldo is essentially correct. The time it takes for the Coupling Coat to cure varies depending on...
Warren (Staff)
-
9 Years Ago
Hi Hanaldo and Warren Thanks for the replys I am in no rush just didn't want to leave it too long !...
Porkster0
-
9 Years Ago
That is correct.
Warren (Staff)
-
9 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search