Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Simple hood
Simple hood
Post Reply
Like
3
Simple hood
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
Hello, i want to make a simple hood for my car. The hood is simular to a volvo 240 hood, large and without any curves/profiles to strengthen the hood. I have seen the tutoiral oon how to make a hood with a inner and outer part. Iam thinking of doing this without the inner part. first a 200gsm carbon mat then a 650gsm carbon mat. To strengthen te hood iam thinking i could lay down a 10cm 5mm/10mm 3dCore reinforcement at the edges of the hood. Then a new 650gsm matt or two 450gsm.
Is this a good idea or is it not worth a try? Making a inner hood skin mould seem to be a lot of extra work.
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Is this for a road going car? If so, I'd recommend making the bonnet in the same way as the factory bonnet is made. The inner skins often have a lot to do with directing energy to crash structures in an impact situation.
You also need to think about how you will mount the hinges and bonnet latch and any other fasteners. Will you be able to align the bonnet properly without an inner skin?
Reply
Like
3
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 49,
Visits: 486
Yes its suppose to be street legal. The car is 50years old so "
directing energy to crash structures" not shure if this was subject at the time.
I was planning to use hood pins in all four corners and this would be good enough to allign the hood.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search