Hi All!

Me again.

So after a while of planning,  arranging the workshop and almost placing myorder @ £2,000  with easy composites. Ithought I would do some workings out (yes I should have done this before)

So my plan was to make and sell various car body panels andsell them at a cost with a small profit margin. I estimated that the FIAT 500Bonnet in the video would cost about £350 to make, but speaking to easycomposites, it actually costs £600 in core materials.

Now bearing in mind that Carbon bonnets sell for around the£600 mark, I’m wondering whether I need to revisit the drawing board andactually work out if this is a viable business or not?

What are your thoughts? Does anyone on here make parts andhave a good turnover with a margin for profit?

Cheers all

Shane


Shane
-Carbon Amateur-
*Never give up!*
Tags
Reply
Shane1985
Shane1985
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 18, Visits: 175
Thanks guys,

I currently use various couriers for shipping as they offer different prices for different types of shipments, like Hanaldo said you really need to shop to find the best deals.

I am not really planning to make bonnets as they are fairly common. My query on the bonnet was merely a benchmark exercise Smile

 


Shane
-Carbon Amateur-
*Never give up!*
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Shane1985 - 10 Years Ago
Warren (Staff) - 10 Years Ago
Shane1985 - 10 Years Ago
Rich (Staff) - 10 Years Ago
Shane1985 - 10 Years Ago
Rich (Staff) - 10 Years Ago
                     :cool: Cheers Buddy
Shane1985 - 10 Years Ago
Fasta - 10 Years Ago
f1rob - 10 Years Ago
morepower - 10 Years Ago
Boozehawk - 10 Years Ago
kidpaint - 10 Years Ago
Hanaldo - 10 Years Ago
Shane1985 - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search