Hi , as the title really. All my parts are small and ideally need one hand to hold the part and one hand on a pollisher. But a 4" grinder type is to big and heavy to use one handed.

At the moment I use a 4" pollisher that I have clamped on edge on the bench, it works but if I catch the part wrong when spinning it fly across the workshop lol!

The best idea I can think is like a 2" air pollisher gun shape hand held thing. But then air isn't a great option for me and can't find one in electric?

Thanks in advance
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
See if you can find something like the Zentool ZEN-12EM. Not cheap but a great piece of kit. You will definitely want a Dual Action type polisher for doing fiddly little bits. 
carbon man
carbon man
Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Hi cheers, it does look a good bit of kit. I just hope it's comfortable to you one handed. 
FLD
FLD
FLD
posted 9 Years Ago HOT
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
That does look good!  I've got a range of mostly heath robinson polishers.  I have a big 6" bosch polisher, a 4" and a 2" flexi-pad that has Velcro waffle mops that I use with a hand drill and a polishing wheel on the bench grinder.  I have tried the polishing pads in the dremel but it takes too long!
carbon man
carbon man
Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
I also use a Velcro pad on a cordless drill. But it's a little heavy and awkward to use. I can't seem to find these zen tools in the UK? 
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I use a cheap Black&Decker "Mouse" and an expensive german "Fein" multi-tool -- They both vibrate a lot, so are a bit tiring to use for longer periods.

I've not crossed the line into actual "production" runs of small parts, but I'm still thinking seriously about getting one of the small "Mirka" air orbital polishers-

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search