Does ambient temp and the amount mixed affect the pot life?. I mixed 100 grams catalysed at 1.5% by weight and it went off in the pot in about 5 minutes.

Cheers.
Reply
ECV3
ECV3
Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)
Group: Forum Members
Posts: 30, Visits: 106
Hi Hanaldo, The uni mould guide does not give any temp range or pot life only a cure temp, what is the temp range to mix and apply the gel coat and how long should the pot life be ???

Cheers.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search