deceased10
deceased10
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 29,
Visits: 154
Hey guys so I am fairly new to carbon fibre and I am currently overlaying a dashboard. I seem to have this issue where my piece has small bubbles and sometimes larger ones. I was told to use a heat gun and go over the part to remove the bubbles, is this true? I've done it but I'm not sure it seems to be making it worse. Making is ripply. What is the best way to avoid bubbles?
Reply
Like
2
Reply
carbonfibreworks
carbonfibreworks
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
It may be safer to use a hair drier as the temp from a head gun is considerable.
Regards Chris
carbon fibre works LTD
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Heat gun on overlayed part to remove bubbles?
deceased10
-
9 Years Ago
Heat gun definitely works, but you have to be careful to not hold it too close or have it on too...
Hanaldo
-
9 Years Ago
It may be safer to use a hair drier as the temp from a head gun is considerable. Regards Chris...
carbonfibreworks
-
9 Years Ago
If you are talking about bubbles under the carbon skin then heating it up will only make it worse as...
Fasta
-
9 Years Ago
Allowing the resin to de-gas for a few minutes after mixing and using slow and smooth brush strokes...
MarkMK
-
9 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search