By deceased10 - 6/9/2016 8:51:58 PM

Hey guys so I am fairly new to carbon fibre and I am currently overlaying a dashboard. I seem to have this issue where my piece has small bubbles and sometimes larger ones. I was told to use a heat gun and go over the part to remove the bubbles, is this true? I've done it but I'm not sure it seems to be making it worse. Making is ripply.  What is the best way to avoid bubbles? 
By MarkMK - 6/12/2016 11:13:35 AM

Allowing the resin to de-gas for a few minutes after mixing and using slow and smooth brush strokes can help minimise air entrapment. Also, building up your required thickness in thin coats will help a little too.