Going from CAD files to moulds


Author
Message
bkayyar
bkayyar
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 5, Visits: 22
Hey all,

I am trying to make a mould for a certain carbon fiber part that has been designed using CAD software. Traditionally, polystyrene foam has been used -a negative mould is made in the foam using a CNC cutter, and the surface of the mould is then prepared using layers of epoxy and bondo. The top layer has always been a hand-sanded super-smooth layer of epoxy. Given the amount of labour involved, I am looking for alternative methods. 
Specifically, my idea was to use the CNC to cut the part itself out of the polystyrene foam such that I have a positive mould, which I would then coat with a thin layer of epoxy. I then intend to use the Uni-Mould system, treating the epoxy-covered foam as a regular part, to obtain a negative mould. Any suggestions or reasons this would not work? I am especially concerned about the layer of epoxy on the polystyrene foam reacting with the epoxy-based gelcoat and hindering its release.
Reply
bkayyar
bkayyar
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 5, Visits: 22
The epoxy tooling block seems to be similar to the polyurethane model boards being sold, but I will give it a shot. Thanks!