The shape is relatively simple, although if the vertical is too steep you may need to make it a 2 part mould to aid demoulding. You would also need to consider extra reinforcement around the screw hole areas or consider a different type of fixing as carbon fibre (and composites in general) are not great with point loadings so fixings need to spread the load to prevent them ripping through.