Carbon Fiber Bathtub


Author
Message
Finnluxury
Finnluxury
Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)Supreme Being (345 reputation)
Group: Forum Members
Posts: 50, Visits: 448
One of my latest projects is Carbon Fiber Bathtub. Its made with resin infusion. Photos are not the best, but it looks awesome in reality.

http://www.talkcomposites.com/Uploads/Images/c3b0cbea-bfd5-47b8-a5a7-1f6a.jpg


http://www.talkcomposites.com/Uploads/Images/5897541d-2f8f-43b3-a803-1e2c.jpg
Reply
VVS
VVS
VVS
posted 9 Years Ago HOT
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
That looks superb, must have been fun to lay up.