Carbon Fiber Bathtub
Carbon Fiber Bathtub
Post Reply
Like
5
Carbon Fiber Bathtub
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Finnluxury
Finnluxury
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 50,
Visits: 448
Its currently pure carbon. I wanted to test first what the bathtub will look like, before making it to final strength. I most likely add some Lantor Soric, as using just pure carbon is a bit waste of material, as bathtub will not need ultimate strength.
For the earth bonding tip, I guess I wont need it. In the space where I have this bathtub, has no other electricity than lights.
Renting the mould can be quite difficult, As I assume U r not living in Finland. I can make U a one bathtub in reasonable price.
Reply
Like
4
VVS
VVS
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
That looks superb, must have been fun to lay up.
Reply
Like
3
ajb100
ajb100
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Very cool! Any chance of renting out the mould?
Reply
Like
4
carbonfibreworks
carbonfibreworks
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
It looks great and dont forget the earth bonding when its installed .
Chris
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Very cool!! Is it solid laminate or have you gone for a cored layup?
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
Finnluxury
Finnluxury
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 50,
Visits: 448
One of my latest projects is Carbon Fiber Bathtub. Its made with resin infusion. Photos are not the best, but it looks awesome in reality.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search