Hi everybody,

I've started doing carbon bikes two years ago and we have built about 8 already with very basic production technology. For this year I am planning to build a replica of the famous lotus 108 pursuit bike. Does anyone have an idea about the building process used? It would be nice not just copying the frame, but also doing a replica of the building proces.
I read it is vacuum assisted resin infusion (which we also use for dropouts, so I am familiar with it) using a PU foam core. My question would be - how is the frame split into "halves" or parts during or is it molded as one piece? If it is done in one piece: how is it possible to control resin content in such a process?



regards,

 Alex
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I would suggest watching EC's tutorial videos, as they cover these subjects very well. 
FLD
FLD
FLD
posted 9 Years Ago HOT
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
There was a panorama on it many years ago.  The film showed straight wet-lay but this was HQ fibre products making the very first one for mike burrows.  Might be worth seeing if it's on tinterweb.