Hi guys,




I am using Airtech's pressure strip for making carbon fiber product. It is working really well for creating the fine edges. However, the lead time in the factory is taking so long for purchasing. I want to get some advices and suggestions for other pressure strip.




Thanks,




Brian
Reply
davro
davro
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Interesting idea, I noticed on the page http://www.airtechonline.com/Pressure-Strip

"Pressure Strip is used as an expendable item and discarded after each cure." 







David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search