By Brian - 5/2/2016 2:03:48 AM

Hi guys,




I am using Airtech's pressure strip for making carbon fiber product. It is working really well for creating the fine edges. However, the lead time in the factory is taking so long for purchasing. I want to get some advices and suggestions for other pressure strip.




Thanks,




Brian
By Brian - 5/24/2016 6:58:40 AM

thanks for the suggestion of airpad. do you also happen to know the most used one?