How fast I can start infuse parts from mould, made with unimould system
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Finnluxury
Finnluxury
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 50,
Visits: 448
Hi!
I have usually just made epoxy moulds, So I wanted to ask a question because I am not sure how this unimould system, differents from epoxy based mould. If I dont post cure the mould, how fast I can start making parts from the mould? If I release the mould from the plug, Am I ready to use the mould in next day? or will there be a styrene pockets or something? So basically I am asking how long it takes to have the mould ready for use.
Reply
Like
2
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
They'll be fine straight away. I've made moulds from start to finish in 8 hours and put them to use straight away without issue. Not that I recommend that, no doubt they wouldn't have a very long life, I just did it to get out of a bind with our race car. I
dont use Unimould either, but there won't be a great difference between that and any other quality vinyl ester tooling system.
Basically yes, you can put them to use straight away.
Reply
Like
2
Finnluxury
Finnluxury
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 50,
Visits: 448
I started making my first mould with unimould system. I was shocked how fast the gelcoat started to cure with 2% ratio. Next time i must use 1.5% ratio of hardener. First gelcoat layer did had some clumps now. I hope they will not affect in final mould surface quality. Never had clumps before, so no idea. It started to make clumps under 10minutes.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search