Finnluxury
Finnluxury
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 50,
Visits: 448
Hi!
I wanted to share some photos what we are building. Currently we are super busy to make these parts for stoneleigh kit car show.
Reply
Like
5
Reply
Finnluxury
Finnluxury
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 50,
Visits: 448
Here is few new photos from our local show. The first photo with front end took me 10 minutes to attach over the chassis. Quite fast! Our aim is to have all panels fitted to chassis less than 30 minutes.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Finnluxury Tritium. aka. FLT
Finnluxury
-
9 Years Ago
Good luck! I'm having trouble getting my kitcar recommissioned and ready for the show, and all it...
ChrisR
-
9 Years Ago
What car U are taking to the show? Its for sure that we do not have time to make all the panels for...
Finnluxury
-
9 Years Ago
Its' a Shelsley T2 [img]https://farm4.staticflickr.com/3275/2844662305_656fe5e0c9_b.jpg[/img]
ChrisR
-
9 Years Ago
I will pop over and say Hi at the show as I wonder round. Nice looking project.
Warren (Staff)
-
9 Years Ago
Yes, we've noticed plenty of materials going your way. Best of luck getting everything ready for the...
Matt (Staff)
-
9 Years Ago
Very interesting project, hope it all comes together !! Hope to see you at Stoneleigh, I will be...
davro
-
9 Years Ago
I wanted to inform that Car will not take part of the stoneleigh show, because we had delays with...
Finnluxury
-
9 Years Ago
RE: Finnluxury Tritium. aka. FLT
Finnluxury
-
9 Years Ago
That's a shame, as was looking forward to seeing some of your work
MarkMK
-
9 Years Ago
Bad luck, this composites work always takes longer than expected. Did you give the uni mould a go?
VVS
-
9 Years Ago
Yes, I tried the unimould. I made perfect 3pcs split mould for the roof. It worked perfectly as i...
Finnluxury
-
9 Years Ago
Bonnet panels are not bond together. I will bond them later on, I must remove the temporary yellow...
Finnluxury
-
9 Years Ago
New Plug photos :)
Finnluxury
-
8 Years Ago
More photos
Finnluxury
-
8 Years Ago
Looking good! Are you planning on showing the car at any motorshows this year?
Warren (Staff)
-
8 Years Ago
[quote][b]Warren (Staff) (03/03/2017)[/b][hr]Looking good! Are you planning on showing the car at...
Finnluxury
-
8 Years Ago
Can't wait to see it now everything is coming together!
Rich (Staff)
-
8 Years Ago
Rear diffuser outer and inner plug.
Finnluxury
-
8 Years Ago
...
Finnluxury
-
8 Years Ago
I just released the Front mounting panel from the mould. All composites companies told me that its...
Finnluxury
-
8 Years Ago
That part looks stunning! Well done for the patience to get it right.
Warren (Staff)
-
8 Years Ago
Here is few new photos from our local show. The first photo with front end took me 10 minutes to...
Finnluxury
-
8 Years Ago
looking good
scottracing
-
8 Years Ago
https://www.youtube.com/watch?v=eR8ek1PlpWo
Finnluxury
-
8 Years Ago
One new photo
Finnluxury
-
8 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search