Hi, I've been looking at the pultruded tubes and box sections as a want to make a wing spar using them but i want to be able to slide a centre tube inside two others if you get what I mean. so all I need to know really is; will a 10mm od tube slide into a 10mm id tube? or are the tollerences not accurate enough to allow this?

Thanks, Look forward to a reply, Steve.

There is an art, or rather a knack to flying.  The knack lies in learning how to throw yourself at the ground and miss.  ~Douglas Adams, Hitchhikers Guide to the Galaxy
Reply
Aero Steve
Aero Steve
Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)
Group: Forum Members
Posts: 11, Visits: 20
Thanks for that, I ordered up the tubes.

you were sure right when you said they didn't really need any sanding, although i'm pretty sure that they would have worked straight out the box I literally spent no more than a minute with 1500 wet and dry and they slid together really smooth, thanks for your help so far

Steve.

There is an art, or rather a knack to flying.  The knack lies in learning how to throw yourself at the ground and miss.  ~Douglas Adams, Hitchhikers Guide to the Galaxy
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search