Hi Folks,
I am a new member and live in the USA. I have a problem with my resin mixture going off too soon. I bought (medium) speed resin. It is supposed to have about 25-30 min pot life at 80deg. I live in South Carolina, and 80deg is pretty cool this time of year! The temp is expected to get to close to a 100deg this weekend, just as I plan on doing a lamination project. My question is how can I slowdown the reaction of the resin? I will be working outside, so no A/C to help. Would placing the resin in a fridge before mixing help? I know I can't reduce the hardener ratio to slow it down. Any ideas?
Reply
Gary
Gary
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 2, Visits: 19
Thanks very much for the advice Guys. Great info. I plan on starting a first light, so should be cooler, and I will dived resin into smaller containers. First time I worked on CF I had a "runaway" in only a 16oz pot that was pretty full. I thought What the hell?
Edited 14 Years Ago by Gary
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search