Thanks Matt,
Ok I get what your saying about laying it down, Now that I know .5mm is the max then I can better/quicker gauge where I should be at and lay it down a little faster. I was thinking much thinner, then kinda kept trying to ad a lil more add a lil more and I ended up building the speckles up. I'm just gonna Jam it on thier quick. How many passed to you typically do over the same spot? Just one? 1.5?
I am thinking that Laying down the GC50 is even trickier when working with small parts under 1ft by 1ft.
I will be back with pics'