Here it is boys, something I like to think as the last step in getting a perfect part!

After stepping into the clearcoating/painting business I can tell you, with or without a paint both it is a total PITA. I cant stand clear coating a part after de moulding, then the clearcoat gets wavy or a bug in it. then i san and polish, still not perfect.

I'm starting to learn this real fast; the key to a perfect part, is taking a mould from a perfect part and polishing it there. I plan to make some really perfect molds, then try this.

 

http://www.easycomposites.co.uk/Images/products/medium/GC50_epoxy-compatable-ploy-gel-1kg.jpg

 

The site says you can brush it on, we for my size parts that would be really connivent. Now matter what the surface of the part will be perfect but if your paint strokes on the back are to thick you may see your weave get a little wobbly.

When making parts smaller than ".5 meter" I think my cup gun is a bit much? think an air brush system would work?

 



If Brute Force Isn''''t working your not using enough...
Replies
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hey guys,

For when I need a smaller amount of GC50, I made me a smaller cup adapter, so I dont waste a big cup.
Pictures here under.

I know how the G100 works and how easy it is to clean, so I chose to adapt it rather than buying another big tip airbrush-kinda-stuff that i would need to learn how to set perfect every time.

While I was at it, I also made a bigger tip (6.5mm) for other gelcoats, as my bigger tip was previously 4.7mm (which works well for GC50).

For those who cant access a lathe, I think making it made would not cost more than buying another smaller airbrush-like gun with 5mm tip, if such thing does exist anyway.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Attachments
G100 Small Cup [640x480].jpg (522 views, 41.00 KB)
G100 Small Cup (1) [640x480].jpg (465 views, 19.00 KB)
Edited 13 Years Ago by Joe
Dave
Dave
Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)
Group: Forum Members
Posts: 48, Visits: 253
Definitely will be giving this a try for some of my products!

Joe (12/07/2012)
Hey guys,

For when I need a smaller amount of GC50, I made me a smaller cup adapter, so I dont waste a big cup.
Pictures here under.

I know how the G100 works and how easy it is to clean, so I chose to adapt it rather than buying another big tip airbrush-kinda-stuff that i would need to learn how to set perfect every time.

While I was at it, I also made a bigger tip (6.5mm) for other gelcoats, as my bigger tip was previously 4.7mm (which works well for GC50).

For those who cant access a lathe, I think making it made would not cost more than buying another smaller airbrush-like gun with 5mm tip, if such thing does exist anyway.


Nice stuff Joe, i do envy you having access to a lathe!

Dave.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Carbon Tuner - 13 Years Ago
Dave - 13 Years Ago
Carbon Tuner - 13 Years Ago
Paul (Staff) - 13 Years Ago
stuart321 - 13 Years Ago
Matt (Staff) - 13 Years Ago
pk_090 - 13 Years Ago
Matt (Staff) - 13 Years Ago
Carbon Tuner - 13 Years Ago
Matt (Staff) - 13 Years Ago
marc37i - 13 Years Ago
Carbon Tuner - 13 Years Ago
marc37i - 13 Years Ago
Warren - 13 Years Ago
Carbon Tuner - 13 Years Ago
Warren - 13 Years Ago
Carbon Tuner - 13 Years Ago
Carbon Tuner - 13 Years Ago
Matt (Staff) - 13 Years Ago
Carbon Tuner - 13 Years Ago
Matt (Staff) - 13 Years Ago
fgayford - 13 Years Ago
Carbon Tuner - 13 Years Ago
Matt (Staff) - 13 Years Ago
marc37i - 13 Years Ago
Matt (Staff) - 13 Years Ago
marc37i - 13 Years Ago
Matt (Staff) - 13 Years Ago
Carbon Tuner - 13 Years Ago
Kevin-Lee - 13 Years Ago
Carbon Tuner - 13 Years Ago
NikCFC - 13 Years Ago
Joe - 13 Years Ago
Dave - 13 Years Ago
Carbon Tuner - 13 Years Ago
Carbon Tuner - 13 Years Ago
Carbon Tuner - 13 Years Ago
mikew - 13 Years Ago
Matt (Staff) - 13 Years Ago
mikew - 13 Years Ago
Matt (Staff) - 13 Years Ago
Carbon Tuner - 13 Years Ago
Carbon Tuner - 13 Years Ago
Matt (Staff) - 13 Years Ago
Carbon Tuner - 13 Years Ago
wozza - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search