You can add styrene up to about 7 % of the resin/gel but you'll find that at that ratio it might start to affect the resin/gel (causing it to become more brittle when cured) so try to add as little as you can get away with.
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|