Group: Administrators
Posts: 214,
Visits: 782
|
in theory as long as you have a 100% even coat of wax in one hit then fine. However usually you do multiple layers to garuntee that 100% coverage.
With a chemical release agent its much quicker to apply and only needs 1 or 2 coats per pull from the mould if youre doing infusion.
|