Cool, yes I think I will try that next. I did post somewhere around here that the wax and pva coating is starting to be the most imperfection problems..
I have been cutting back on waxing, was like 5, then 3 then 2 coats. When your mould is real shiny its easy to see the wax. Also after the wax a light coat of pva.
As far as waxing If I can see the haze over the mould I'm good right? I think I could get away with waxing one time and a quick coat of pva. the thinnest coat of wax will work as long as its evan and completely covered??
Wish I would bought this stuff when I was ordering the other day.... The shipping to USA drives me insane!!!!!!!!!!!!!
Next round I guess...