Group: Forum Members
Posts: 468,
Visits: 2.7K
|
You need some sort of key on the aluminium. Another option is a PU primer which is a runny PU adhesive. This gets into the nooks and crannies of the alu surface to give a good bond. I use 'winbond' from a screen fitter with tiger seal and it works a treat.
|