Custom Carbon fibre case from scratch.


Author
Message
rudger
rudger
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 1, Visits: 8

Hi I'm a complete carbon fibre newbie so please bare with me. I'm looking for some adviceregarding creating a custom case from scratch. I do not have a case similar to anythingI want which is why I'm planning to make a case out of carbon fibre.

the case I would like to make needs to have internaldiameters of around 142cm Long, 16cm Wide, 6cm High. to allow for foam padding myquestions are.

1. roughly how thick do the layers of carbon fibre need tobe to provide protection to avoid damaging the item inside when stepped on andnot to warp if the case is leant diagonally - when I carry it in my car.

2. what would be the best way /material to make a mould outoff - I would ideally like all the outer corners to be curved so I feltMDF/wood may not be suitable. I'm not too concerned about the appearance of theinner corners of the case as it will not be seen however the lip where the case2 halves of the case join together will be seen so I would like them to be veryclean and tidy.

3. I plan to fit Hinges and locking fasteners onto the longestedges of the case I guess that if I made the mould 3cm high I could use themould twice so the top half and bottom half would be the near identical. isthis possible or would I have to make 2 separate moulds?

4. as stated in question 3 I will need to fit hinges andlocking fasteners does anyone on the forum have experience or can recommend asupplier also advise on the best way to fix them to the case.

5. roughly what materials and quantities will I need toorder.

wow reading all the above makes me realise how much of anewbie I may be. Thanks in advance

Rudger.


Reply
Carbon Tuner
Carbon Tuner
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 104, Visits: 422

Well heres what my approach would be;

 

1. roughly how thick do the layers of carbon fibre need to be to provide protection to avoid damaging the item inside when stepped on and not to warp if the case is leant diagonally - when I carry it in my car.

4-5 layers of the heaviest 2x2 twill.

 

 

2. what would be the best way /material to make a mould out off - I would ideally like all the outer corners to be curved so I felt MDF/wood may not be suitable. I'm not too concerned about the appearance of the inner corners of the case as it will not be seen however the lip where the case 2 halves of the case join together will be seen so I would like them to be very clean and tidy.

make half the case out of wood, sand it down shape it and fill in al gaps with body filler, then primer and make smooth. Then make a mold off that.

 

3. I plan to fit Hinges and locking fasteners onto the longest edges of the case I guess that if I made the mould 3 cm high I could use the mould twice so the top half and bottom half would be the near identical. is this possible or would I have to make 2 separate molds?

read #2 answer

 

4. as stated in question 3 I will need to fit hinges and locking fasteners does anyone on the forum have experience or can recommend a supplier also advise on the best way to fix them to the case.

I would checkout the Structural Adhesives on easy composites; https://www.easycomposites.co.uk/adhesives

get some of that, glue a metal bracket to that and mount your hinges there.

 

 

5. roughly what materials and quantities will I need to order.

Im american I cant convert, to lazy but based on a 4-5 layer setup I think by going to the website you could figure it out or maybe someone from UK can help.





If Brute Force Isn''''t working your not using enough...
Edited 13 Years Ago by Carbon Tuner