Hello all,
 I wrote late last year and asked if assistance could be give to make a mould for a F3 defuser. race car. and that a couple of attempts  had been made with a sad ending, and too the rubbish heap they went.

I have made a mould off the old defuser using glass etc.  and I thought I would use this as a mould for the defuser however, my troubles began when I used foam and carbon fiber to form the underneath ribs and when it was pulled down with the vacumm bagging process the ribs become out of shape under pressure.

I am no expert  with this process and I would appreciate assistance?.
Do you have to have  a split mould top and bottom to form the mould.

I would appreciate your comments, I will take a photo tomorrow and post it until then
Thanks
Sam
Reply
davro
davro
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Dropbox does not allow direct hotlinking so you can't even use the image tags.
I just upload to google photos and hotlink directly from there cache Wink

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
sam - 9 Years Ago
sam - 9 Years Ago
scottracing - 9 Years Ago
sam - 9 Years Ago
Ronny - 9 Years Ago
ChrisR - 9 Years Ago
davro - 9 Years Ago
scottracing - 9 Years Ago
MarkMK - 9 Years Ago
sam - 9 Years Ago
Ronny - 9 Years Ago
MarkMK - 9 Years Ago
davro - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search