Best release agent for plug


Author
Message
Paul M
Paul M
Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)
Group: Forum Members
Posts: 18, Visits: 79
Hello,making a plug for a motorbike tank from the original tank.
I have sanded it down and used filler primer as there were a few
small dents and scratches,they have all been filled and smoothed,
next I will polish the top half.I have got mould release wax,
semi-permanent release agent and P.V.A.release agent.Which off
these would work best on the filler primer.

   Cheers Paul
Attachments
IMAG0580.jpg (697 views, 594.00 KB)
IMAG0583.jpg (618 views, 617.00 KB)
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
If you are new to this and you have the ability to spray the PVA, go for this. It is the most forgiving option, if not quite the best. 

If you've got a bit of experience, and the primer filler is a well cured 2k, use the semi-perm. Do a test before committing to the whole mould. 
Paul M
Paul M
Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)
Group: Forum Members
Posts: 18, Visits: 79
Thanks for the reply,I have never used filler primer before,so not to sure
what works best wax,P.V.A. or semi perm.Will do as you say and do a test
first.Will most probably us wax and P.V.A. to make the mould as I now this
works and have had no problems before with primer.For making the part I
will use the semi-perm.
I have been fibreglassing on & off for about 20 years,new to vacuum infusion
and using semi-permanent release.Will have a lot of questions as I go along,
some will be simple to most people on here,but to me they will be confusing.
As long as I learn I'll be happy.


   Cheers Paul

Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Don't think anyone here is worried about answering any questions you have, no matter how straight forward it is. That's what forums are for, and this one is particularly helpful, so don't hold back! 

I think the best rule is if you are unsure of any of your materials, then do a test in an area that isn't going to ruin the part if something goes wrong. If that isn't possible, stick to PVA. It's the most reliable release agent you can use. 
Chris Scott
Chris Scott
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 20, Visits: 235
Anytime I have a plug/pattern made of different compositions (wood, primer, unknown plastics, etc) I just use PVA to be safe. I spray it on and it leaves an amazing finish. Eliminates risk with no set back (in my experience at least).
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search