XCR Skinning process


Author
Message
Lenny
Lenny
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 16, Visits: 58
I would like to carbon skin a part and I have a question regarding the 'tack' time before applying the carbon.  The part I want to skin is quite large and has complex surfaces.  I don't want the resin base coat to be really tacky as once you lay the carbon it is very difficult to manipulate into position within damaging the weave pattern.   Therefore, could you lay the carbon earlier, so that the base coat is not so tacky and allows you to manipulate the carbon ? The process states 1-2 hours, but laying on after 10-30 minutes, would this cause any issues ?
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Sounds like you need to give the black basecoat a good stir in the container it came in .. maybe some of the pigment has "settled"

I never buy or use the black bascoat, so cannot testify as to how "opaque" it is or how well it covers.. I make my own, by adding apprx.. (very approximately .. Whistling) 5 % of EC's "West & Senior epoxy colour dispersion" in black ..  That covers even the brightest colours on the part ..  Very thin layers of basecoat will be a bit transparent ..



"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Lenny - 10 Years Ago
matthieutje65 - 10 Years Ago
Warren (Staff) - 10 Years Ago
Matt (Staff) - 10 Years Ago
67redrocket - 10 Years Ago
Dravis - 10 Years Ago
Lenny - 10 Years Ago
Warren (Staff) - 10 Years Ago
Warren (Staff) - 10 Years Ago
JonS - 10 Years Ago
Warren (Staff) - 10 Years Ago
JonS - 10 Years Ago
Dravis - 10 Years Ago
Dravis - 10 Years Ago
Warren (Staff) - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
meir - 10 Years Ago
Davidcorrado - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
Umut Can Kizilray - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search