Peelply texture


Author
Message
AlessandroPA
AlessandroPA
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 26, Visits: 301
Just a tip from the group: when using the vacuum bagging, does anybody use only the perforated film and the breather? Adding to these,I use also the peelply (as it could be as usual) closer to the carbon fiber, but when out of the mould the finish is with the texture of the peelply. 
Do you think I could use only the film and the breather, so to have the carbon with a more glossy finish?
Thanks for your help 

Alessandro 
Replies
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
There's a product called infuply which is perf release file with mesh bonded to it removing the need for peel ply. It woks pretty well, but as above, the finish is worse imo that peel ply
AlessandroPA
AlessandroPA
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 26, Visits: 301
Thanks for your suggestion. Anyway, I tried to lay up the only film, but the final result has been really horrible (fortunately I tried to apply it only by hand, no vacuum)!
So, I'm scratching the last layer and I will back to lay up the "normal" procedure peelply-film-breather Smile

ajb100 (30/01/2016)
There's a product called infuply which is perf release file with mesh bonded to it removing the need for peel ply. It woks pretty well, but as above, the finish is worse imo that peel ply