Group: Forum Members
Posts: 592,
Visits: 1.9K
|
Yes you can, but it will be an uneven and slightly bumpy surface, and not really "glossy" -- I find that peel-ply, when removed makes for a very nice even surface, that can be coated very easily with clear coat or just brushed carefully with epoxy, making a much nicer surface. Also, when the peel-ply is removed, the surface can be sanded a bit down very easily, and you will use less coating.
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|