Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Surface requirement for mould making
Surface requirement for mould making
Post Reply
Like
4
Surface requirement for mould making
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Makerbot
Makerbot
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 126
Hi,
I am planning on making some car panel moulds, can you tell me if I can make the mould from panels in primer or do they need to be painted?
Thanks
Reply
Like
4
Reply
Makerbot
Makerbot
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 8,
Visits: 126
matthieutje65 (22/01/2016)
If possible I allways avoid primer/bondo and so on to make a mould of...I always topcoat it or clearcoat it with a 2K to make sure it demoulds well...
It's in the nature of these products to absorb (normally paint) coming on top so not ideal to make a mould on with the risk of it sticking...with a topcoat or clearcoat, 2K that is fully cured!, you should never have any problems with demoulding with the chemical release agent
Thanks Matthieu, more to consider for the effort/result mix.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Surface requirement for mould making
Makerbot
-
9 Years Ago
Professionally sprayed primer from a 2 pack system will usually be fine once fully cured. You should...
Warren (Staff)
-
9 Years Ago
[quote][b]Warren (Staff) (21/01/2016)[/b][hr]Professionally sprayed primer from a 2 pack system will...
Makerbot
-
9 Years Ago
I mould from primered surfaces (2 pack) and I find the primer takes a sprayed coat of PVA release...
FLD
-
9 Years Ago
[quote][b]FLD (21/01/2016)[/b][hr]I mould from primered surfaces (2 pack) and I find the primer...
Makerbot
-
9 Years Ago
If possible I allways avoid primer/bondo and so on to make a mould of...I always topcoat it or...
matthieutje65
-
9 Years Ago
[quote][b]matthieutje65 (22/01/2016)[/b][hr]If possible I allways avoid primer/bondo and so on to...
Makerbot
-
9 Years Ago
Been looking into this recently and do not recommend fill in any way as it comes out of the part and...
VVS
-
9 Years Ago
[quote][b]VVS (26/01/2016)[/b][hr]Been looking into this recently and do not recommend fill in any...
Makerbot
-
9 Years Ago
I think you guys are misunderstanding how a primer works. Primers don't absorb anything, they are...
Hanaldo
-
9 Years Ago
Actually primer is porous. Thats why they require a top coat as a color and protective layer. You...
kidpaint
-
9 Years Ago
I do believe people have long confused the hygroscopic nature of some primers with porosity. Just...
Hanaldo
-
9 Years Ago
Hanaldo, Very well put, your advice is always on the ball. You are an asset to this...
The Fibreglass King
-
9 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search