Hi folks,



As per the thread title ........  I'm not sure if what I have bought from EC will be fine for what I am trying to accomplish.

I purchased some 'Vac-Cast' Epoxy casting resin as I read it was ideal for a tooling plug as it was an aluminium filled epoxy casting resin resistant to heat.  I've searched on the forum on how to use it ( and on YouTube ),  but can't find anybody that has used it !

I did find however,  many casting tutorials on the net but they were for liquid Latex and others.  Am I to assume it's exactly the same procedure ?  I have also read some of the tutorials on here,  but the guide very quickly deviates to mould construction for the use of vacuum infusion for carbon fibre parts.

I simply need to pour the mixture into a vacuum formed part. Leaving me with a 'male' plug so I can vacuum form many other parts just like my original.



Any information greatly received as I'm really stuck as to which direction I need to go.







Thanks guys.









TURK
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi TURK,

Sorry for the delay in getting back to you but I won't always be the quickest to respond to technical support issues due to the daily routines of running the business. Our technical support guys can be emailed directly on technical@easycomposites.co.uk and they will always get right back to you.

In response to your questions;

will pattern coat primer stick to wood ?
Yes, Pattern Coat Primer will definitely stick to wood. Pattern Coat Primer is, essentially, a polyester resin. If you have any experience of polyester resins then you'll know that they will soak into and bond well to wood, Pattern Coat Primer is no different.

However, looking at your post, I'm not sure that you actually mean Pattern Coat Primer. I think you might mean the Vac Cast Epoxy Casting Resin; this is a totally different product although the answer would be the same because Vac Cast is an epoxy and epoxy also sticks to wood.

If I 'block-out' the underside of the resin mold with wood to save on resin, will I be able to remove the wood block once the resin has cured  ?
Yes, as mentioned above, the epoxy resin of Vac Cast would also stick to wood. To prevent the Vac Cast from bonding to the wood you could go for a basic (but fairly reliable) method of wrapping the wood with brown parcel tape. This type of tape is usually polypropylene and if it is then the epoxy won't stick to it. You can test a small area first to make sure. If you want a more professional approach then you could wrap the wood in Unperforated ETFE Release Film which the resin certainly won't stick to.

Also, the pattern-coat primer and hardener is a 100:6 mix ratio -  what does that mean ?
Again, I'll assume you mean Vac Cast (not Pattern Coat Primer which uses MEKP as a catalyst at a mix ratio of 2%)....
A mix ratio of 100:6 means 100 parts (by weight) of the Vac Cast resin should be mixed with 6 parts (by weight) of the Vac Cast hardener. Put simply, for every 100g of resin you need 6g of hardener.

Say I need 1904 grams of resin,  how much hardener would I use ?  

If you had 1904g of resin then you know you need 6g of hardener for every 100g of resin so 1904/100=19.04; 19.04 x 6 = 114.24g of hardener (or just calculate 1904*0.06).

I hope this helps and, once again, sorry I didn't get back to you right away. It would be great if I could always do this Smile

Matt 

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TURK - 9 Years Ago
matthieutje65 - 9 Years Ago
TURK - 9 Years Ago
matthieutje65 - 9 Years Ago
TURK - 9 Years Ago
matthieutje65 - 9 Years Ago
TURK - 9 Years Ago
Matt (Staff) - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
Matt (Staff) - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
fgayford - 9 Years Ago
TURK - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search