Hi folks,
As per the thread title ........ I'm not sure if what I have bought from EC will be fine for what I am trying to accomplish.
I purchased some 'Vac-Cast' Epoxy casting resin as I read it was ideal for a tooling plug as it was an aluminium filled epoxy casting resin resistant to heat. I've searched on the forum on how to use it ( and on YouTube ), but can't find anybody that has used it !
I did find however, many casting tutorials on the net but they were for liquid Latex and others. Am I to assume it's exactly the same procedure ? I have also read some of the tutorials on here, but the guide very quickly deviates to mould construction for the use of vacuum infusion for carbon fibre parts.
I simply need to pour the mixture into a vacuum formed part. Leaving me with a 'male' plug so I can vacuum form many other parts just like my original.
Any information greatly received as I'm really stuck as to which direction I need to go.
Thanks guys.
TURK
By TURK
-
4/14/2016 7:35:19 PM
Excellent link that 'Freemansupply' Fred ........ many thanks.
I had seen some of their how-to videos on youtube, but some of their articles are very good.
TURK