Generally speaking for our Fast Cast and the West and Senior pigment dispersions you are looking at approximately 10% by weight to get a good even colour.
Of course, any additives will effect the properties of the resin to an extent, but at the levels we are talking about, the weakening will not be significantly noticeable.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|