Thanks for your help Smile
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Generally speaking for our Fast Cast and the West and Senior pigment dispersions you are looking at approximately 10% by weight to get a good even colour.

Of course, any additives will effect the properties of the resin to an extent, but at the levels we are talking about, the weakening will not be significantly noticeable.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
VVS
VVS
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Moderators
Posts: 226, Visits: 334
Hi Brian,

Is there no percentage loading given for the colour buy the manufacturer.
It won't make the part brittle but will affect the structure of the finished part of you over pigment.
brimcel
brimcel
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 2, Visits: 8
Hi,
Hello I'm a newbee at this.
How much pigment do I add to Fast Cast resin ?
Also does the more pigment I add make the final part more brittle ?
Cheers Brian,
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search