I make a few parts in cheapo GRP.  I have no shame!!  I've made some parts recently and I've found the open surface has remained tacky although the laminate has cured.  I catalysed at 3% as normal but the resin I use (East coast) used to be blue and is now brown.  Could it be the resin blend or have I started doing something wrong?

Any ideas on if I can salvage the parts with a solvent wipe or something similar?
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Answered my own problem, they are bin-bound due to a batch of resin.