			            I have used the same type of Birch with the striping from fungus attacks (thats what it is !!)  The wood is not nearly as stable as "clean birch" so I would recommend "stabilizing" it with vacuum and infusion resin when shaped and sanded down .. then sand down this and apply coating resin, or better still get someone to clear coat it with 2 comp. polyurethane  (Car paint shop..)                
			            
  				