OK so I did a search but couldn't find an answer, I've done my first mould now plan on trying to get a perfect surface is it best to use the wet and dry paper dry or with soapy water like you would with car paint?

What grade should I start with the surface is good already just has some scratches from the paint in places 

Thanks Paul 
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
if its just light scratches, then you should be able to use 1000wetndry and then polish from that point.
got any photos?
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
Here's some these are the worst bits
http://www.talkcomposites.com/Uploads/Images/42567220-6fe5-4858-b8d0-701a.jpg




Attachments
20151008_190835_zpswvmlzflc.jpg (447 views, 4.00 MB)
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
http://www.talkcomposites.com/Uploads/Images/d9f972f2-9e0b-407f-895f-fe43.jpg
Scratches
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Treat it the same as if you were sanding car paint, you will find its pretty hard stuff though so you need to renew the paper more often than paint.