Hi folks,
I am trying to recover a Stratocaster that I rubbed back to wood using Coating Resin to get back to a good surface finish before painting.

I am a complete newbie to the use of epoxy resins and now I fear that I have messed it up !! Blink

I mixed up the two parts as instructed on the bottles, and spread it liberally - probably too thickly actually.

that was 2 days ago and now the surface remains slightly sticky, which worries me a lot !

I have a horrible feeling that it isn't going to cure properly, or will it eventually harden up enough for me get in there with some abrasive and prepare it for a final coat?

If not, I guess I will have to scrape it all off and start again...that will the 4th time, having tried the primer/filler, topcoat, clear coat route 3 times and realised that the wood quality is so bad it was never going to cover well.

Incidentally, Fender use epoxy resin as a grain filler so I was hoping to emulate the factory process.

What say you?

Cheers
Dave

Dave the Luthier
Reply
AxShack
AxShack
Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)
Group: Forum Members
Posts: 4, Visits: 20
great stuff, many thanks for the pointers there...just off to the workshop to see if it is ok

D

Dave the Luthier
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search