EC infusion epoxy works very well for sealing plaster .. It will not react with anything, and it will be partly absorbed into the plaster .. just brush on a liberal coat .. 2. coat can go on when the first cures to a tack..
Then you can sand and smooth some more, and use other stuff on top ..