Does anyone have any tips to help remove vac bag tape, especially from a peel ply surface. I have been adding some reinforcement to an existing CFRP structure and thus have been sealing vac bag film over the new bits of carbon. I have pulled all the bagging film and the bulk of the tape off but there are still some small amounts of tape stuck to the original surfaces.
|