Hi!
One of my customers wants 250 degree celsius heat resistant covers for ultra light airplanes. He wants like a lot of them. Normal high temp resins perish at 180 so I would hit prepreg, but isn't that too hot even for it? what do you think? I couldn't find any data sheet about prepreg hdt after curing.
Thanks

~~~Everytime I hear sound of demoulding part I have eargasm~~~
Replies
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
You need to use some kind of heat shielding.

link to typical thing used in motorsport

http://www.demon-tweeks.co.uk/motorsport/heat-shielding-protection/pitking-products-cool-tape
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
it is more like the carbon is a heat shield itself and it directs the air over the cylinder fins to cool it as it is AC engine

I found Hexcel M-81 which could withstand up to 200 degrees but with complicated curing scheme and I quess it is not out of autoclave one Sad

http://www.hexcel.com/Resources/DataSheets/Prepreg-Data-Sheets/M81_eu.pdf


~~~Everytime I hear sound of demoulding part I have eargasm~~~