Group: Forum Members
Posts: 23,
Visits: 163
|
I think people are getting off track... with the shapes and variables (twill/plain, low/high humidity, post cure, etc.) because sheet metal's rigidity is affected by shaping. If "you" had to make/replace a given (your choose) steel hood and make it the same...I.E. shape and hood frame out of 100% CF AND one out of 100%E glass what would be the wt cloth and # of layers you would use. I know with the variables no one will/can give an "exact" # for a 1 to 1 ratio, so lets say a range or minimum( do in a lab by a machine) to a DYI guy in his backyard for comparison sake. For example thickness of fiberglass to make a 2"x 4" box tubing 4ft long that would as strong or stronger (in every load direction) than one made of 1/8"mild steel. There "is" an equivalent # out there that would always give an "atleast as strong" for an equivalent of a different material.
|