I've been building my first plug for the air conditioning housing on my Marcos Mantula. While I'm quite happy with the way it has turned out in general I am finding the application of the pattern coat primer to be more difficult than shown in the Easy Composites video. I've tried using a brush and a roller, but can't seem to get to the stage where it only needs minor sanding. There always seems to be new imperfections with each coat.

Maybe the working time is too short. I try to mix accurately using digital scales, but never seem to get a consistency that allows the brush or roller marks to flow out. Any ideas what I'm doing wrong?

Thanks
Edited 11 Years Ago by Ian Mantula
Reply
TURK
TURK
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 101, Visits: 662
Hanaldo (12/11/2015)
Why are you not filling the low spots with body filler? 




Hi Hanaldo,

Good question,  normally that would be the way to go ........  but at the stage where I'm currently at ( 20 odd coats of pattern-coat primer ) I can't ....... or rather I'm afraid to 'undo' all the work I've already done.

If I were hand laying or bagging carbon fibre I think it wouldn't matter,  but I'm using my plugs as 'tooling plugs' for vacuum forming.  As that process involves subjecting the plugs to high heat,  the build-up of pattern-coat primer acts as a shell if you like,  as pattern-coat primer has aluminium in it.  If I go and fill the low spots with body filler now,  I'll only create weak spots in that heat resistant 'shell'.  I've had issues in the past with thin layers of polyester filler cracking due to heat,  so I really don't want to risk it at this stage,  so I'm having to use the pattern-coat primer as a filler as it were.



As the OP was commenting on the pattern-coat primer as a product,  I thought I had to pitch-in with my findings ........  that is to say,  it doesn't actually do what it pertains on the Data Sheet !

It's seen as a very high viscosity primer almost like syrup,  so a couple of coats of pattern-coat primer and you're done. 
I can assure that is not the case ......... it may become thicker in the last two minutes of it's pot life,  but the initial mixture is more like regular emulsion paint.  



I had to build up my plugs by 2mm as they have to fit inside a bracket,  so with the Data Sheet I concluded that 2 coats of 1mm each would be enough ........ it's taken 20 coats to get to that stage !



Don't get me wrong,  I'm not complaining about the actual product as it's doing what I want it to.  But the Data Sheet information is very misleading  Angry


Next time I'll be looking for a different product,  something much thicker but also very durable as I have to able to vacuum form many many parts from it.




TURK

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Ian Mantula - 11 Years Ago
Dravis - 11 Years Ago
Olivier - 11 Years Ago
MarkMK - 11 Years Ago
matthieutje65 - 11 Years Ago
Ian Mantula - 11 Years Ago
MarkMK - 11 Years Ago
MarkMK - 11 Years Ago
Hanaldo - 11 Years Ago
MarkMK - 11 Years Ago
Hanaldo - 11 Years Ago
TCS - 11 Years Ago
TURK - 11 Years Ago
Hanaldo - 11 Years Ago
TURK - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search