Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
thats interesting Mark, still have a video to make about the primer and gloss on plugmaking I'll keep that in mind while making the video and trying the materials for the first time
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
MarkMK
MarkMK
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 338,
Visits: 2K
Even with spray application you need to bargain on a fair bit of flatting to get it nice and smooth. I now use a half and half mix of primer and gloss, usually a couple of coats to give plenty of material to flat back. The resultant satin finish that transfers to the mould is then fairly easy to bring up to a good shine with the machine polisher and compound.
I just find that this combination provides the best of both worlds in terms of hard finish and (fairly) easy sanding
Reply
Like
4
Olivier
Olivier
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 89
Hi,
I used EC Pattern Coat Primer and HI-Gloss to make this plug.
After lots of coats I gave up and finished it with the HI-gloss then sanding and polishing to make moulds with EC Uni-Mould range of products.
I gave up probably because the part made of plaster and filler was too rough and I sanded trough the primer each time. So it took a long time to have a decent plug.
At first I wanted a nice uniform black plug but...
Finally plugs were fine and moulds were easy to build.
Hope this helps
Attachments
image.jpg
(
857 views,
687.00 KB
)
Reply
Like
4
Dravis
Dravis
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
I had the same problem with my last batch of EC Pattern Coat primer ... I thought it might be the temperature in my workshop being a bit low .. So I heated the Primer coat a bit, to maybe 25 degrees . That helped a bit, but I still had quite a bit of sanding to do..
The gloss pattern coat was a bit better, but still had brush marks and uneven surface i some areas .. They are good products, but not "perfect"
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
4
Ian Mantula
Ian Mantula
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 24,
Visits: 668
I've been building my first plug for the air conditioning housing on my Marcos Mantula. While I'm quite happy with the way it has turned out in general I am finding the application of the pattern coat primer to be more difficult than shown in the Easy Composites video. I've tried using a brush and a roller, but can't seem to get to the stage where it only needs minor sanding. There always seems to be new imperfections with each coat.
Maybe the working time is too short. I try to mix accurately using digital scales, but never seem to get a consistency that allows the brush or roller marks to flow out. Any ideas what I'm doing wrong?
Thanks
Ian
Marcos Mantula blog
Edited
11 Years Ago by
Ian Mantula
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search