I've been building my first plug for the air conditioning housing on my Marcos Mantula. While I'm quite happy with the way it has turned out in general I am finding the application of the pattern coat primer to be more difficult than shown in the Easy Composites video. I've tried using a brush and a roller, but can't seem to get to the stage where it only needs minor sanding. There always seems to be new imperfections with each coat.

Maybe the working time is too short. I try to mix accurately using digital scales, but never seem to get a consistency that allows the brush or roller marks to flow out. Any ideas what I'm doing wrong?

Thanks
Edited 11 Years Ago by Ian Mantula
Reply
Olivier
Olivier
Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)Supreme Being (216 reputation)
Group: Forum Members
Posts: 26, Visits: 89
Hi,
I used EC Pattern Coat Primer and HI-Gloss to make this plug.
After lots of coats I gave up and finished it with the HI-gloss then sanding and polishing to make moulds with EC Uni-Mould range of products.

I gave up probably because the part made of plaster and filler was too rough and I sanded trough the primer each time. So it took a long time to have a decent plug.
At first I wanted a nice uniform black plug but...
Finally plugs were fine and moulds were easy to build.

Hope this helps


Attachments
image.jpg (857 views, 687.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Ian Mantula - 11 Years Ago
Dravis - 11 Years Ago
Olivier - 11 Years Ago
MarkMK - 11 Years Ago
matthieutje65 - 11 Years Ago
Ian Mantula - 11 Years Ago
MarkMK - 11 Years Ago
MarkMK - 11 Years Ago
Hanaldo - 11 Years Ago
MarkMK - 11 Years Ago
Hanaldo - 11 Years Ago
TCS - 11 Years Ago
TURK - 11 Years Ago
Hanaldo - 11 Years Ago
TURK - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search