Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Uni-mould and neighbours
Uni-mould and neighbours
Post Reply
Like
2
Uni-mould and neighbours
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Olivier
Olivier
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 26,
Visits: 89
Hi,
I use Uni-mould and I love it but my neighbour complains because of the smell.
What would be an alternative? EC epoxy mould?
Will EC green epoxy fix my issue?
How to reinforce epoxy moulds? Can I use CSM and IN2?
I plan to make CF infused with IN2 and or without GC50, twaron, prepegs and natural fibres.
Thanks for your advices.
Reply
Like
2
Reply
Olivier
Olivier
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 89
Ok thanks Hanaldo,
I try to sand EC green tooling epoxy (180 - 400 - 800 - 1200 - 1500 - 2000 by hand 3000 and 3M polish compound with a Mirka machine) to test how is it difficult to repair in case a mould needs repair.
I was not able to get a surface as shiny as an untouched mould and the surface is soft but full of tiny little holes.
Ok it was an old pot and I did pay a lot of attention to mixing it because it was just layed on a piece of vacuum bag for a quick test.
Is it something I can fix with degas?
How to get a shiny finish?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Uni-mould and neighbours
Olivier
-
10 Years Ago
I use EC green and IN2 for the majority of my moulds. It is almost vapour less, you can use it in...
VVS
-
10 Years Ago
Just be careful with epoxy. Just because it doesn't have an odour doesn't mean it is totally safe....
Hanaldo
-
10 Years Ago
I've also found the epoxy gelcoat a bit more prone to trapping air bubbles, owing to its thicker...
MarkMK
-
10 Years Ago
Tanks everybody, I Will use epoxy with the same safety tricks as polyester. And I do not use huge...
Olivier
-
10 Years Ago
One of the EC staff may be able to pitch in here, but I suspect that you could use the epoxy tooling...
Hanaldo
-
10 Years Ago
Ok thanks Hanaldo, I try to sand EC green tooling epoxy (180 - 400 - 800 - 1200 - 1500 - 2000 by...
Olivier
-
10 Years Ago
Yeh that's what I mean, it isn't easy. You can probably do a bit better though, for one 180 grit is...
Hanaldo
-
10 Years Ago
The "green stuff" is a b*t*h to polish up, it really will not polish well --- been there many times...
Dravis
-
10 Years Ago
Thank you guys I will buy different EC epoxies and woven FB. Have a great day building all kind of...
Olivier
-
10 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search